Add BrightSurf on Google Email

New coating protects steel and superalloys

03.24.06 | DOE/Pacific Northwest National Laboratory

Researchers at Pacific Northwest National Laboratory have developed a new ceramic-based coating for steel and superalloys that prevents corrosion, oxidation, carburization and sulfidation that commonly occur in gas, liquid, steam and other hostile environments.

The low-cost, easy-to-apply material is available for licensing and joint research opportunities through Battelle, which operates PNNL for the Department of Energy and facilitates the transfer of lab-created technologies to the marketplace.

The new coating bonds with the metal substrate and is "resilient, inexpensive and simple," said PNNL scientist Chuck Henager. Because the coating is fabricated at significantly lower temperatures than typically required for conventional ceramic coatings, the new process also can save energy and reduce harmful emissions, he said.

Researchers created the coating by mixing a liquid preceramic polymer with aluminum metal-flake powders to form a slurry that can be applied to a metal object by dipping, painting or air-spraying. A low-temperature curing process follows, using a commercial Ruthenium-based catalyst that enables polymer cross-linking and dries the slurry to a green state.

The coated steel is then heated in air, nitrogen or argon at 700 to 900 degrees Celsius. The heat converts the green state layer into an aluminum diffusion/reaction layer that permeates surface of the steel and provides an aluminide surface coating on the steel.

According to PNNL Commercialization Manager Eric Lund, the diffusion reaction makes the coating so durable that it can't be chipped or scratched off.

The reaction layer on the surface of the steel is much stronger than an external coating because it is an integral part of the steel, Henager said. This layer develops during use as the coating is heated at very high temperatures, such as those that occur with the heating of pipes in a process facility.

Unlike similar products, the liquid form of the coating can be applied with a spray gun. This feature makes the PNNL coating practical for protecting large areas, researchers said.

For licensing and other business inquiries, contact Lund (509) 375-3764 or eric.lund@pnl.gov .

PNNL (www.pnl.gov) is a DOE Office of Science laboratory that solves complex problems in energy, national security, the environment and life sciences by advancing the understanding of physics, chemistry, biology and computation. PNNL employs 4,100 staff, has an annual budget of more than $700 million, and has been managed by Ohio-based Battelle since the lab's inception in 1965.

4 PHOTOS AVAILABLE:
http://picturethis.pnl.gov/picturet.nsf/f/uv?open&AMER-6MXS3S

http://picturethis.pnl.gov/picturet.nsf/f/uv?open&AMER-6MXRXX

http://picturethis.pnl.gov/picturet.nsf/f/uv?open&AMER-6MXRWT

http://picturethis.pnl.gov/picturet.nsf/f/uv?open&AMER-6MXRQ2

Keywords

Contact Information

Judith Graybeal
DOE/Pacific Northwest National Laboratory
graybeal@pnl.gov

Source

This article is based on a news release from DOE/Pacific Northwest National Laboratory. BrightSurf curates and republishes science news from research institutions worldwide; the original release is linked below.

How to Cite This Article

APA:
DOE/Pacific Northwest National Laboratory. (2006, March 24). New coating protects steel and superalloys. Brightsurf News. https://www.brightsurf.com/news/86GGD2GL/new-coating-protects-steel-and-superalloys.html
MLA:
"New coating protects steel and superalloys." Brightsurf News, Mar. 24 2006, https://www.brightsurf.com/news/86GGD2GL/new-coating-protects-steel-and-superalloys.html.